I have no meeter and my only choice today was inside. Sucks but whatcha gonna do ....................
This was a rebuild for a customer. I made some aluminum baffles the first time that I cryo treated. I wanted to know what would happen. Now I know. lol
The blast ate the shart out of the bore anyway.
Its an all SS can and baffles
http://youtu.be/Www4ccRJSpI
[ame]http://www.youtube.com/watch?v=Www4ccRJSpI[/ame]
From R/L, sr 4140 blast baffle on to the muzzle. I didnt ask how many rounds
I had hoped I was cutting a fat hog with the cryo. I also had a .22 can have the baffles collapse in FA because I was trying to cut them too thin. They work great on a reg. .22 though
This was a rebuild for a customer. I made some aluminum baffles the first time that I cryo treated. I wanted to know what would happen. Now I know. lol
The blast ate the shart out of the bore anyway.
Its an all SS can and baffles
http://youtu.be/Www4ccRJSpI
[ame]http://www.youtube.com/watch?v=Www4ccRJSpI[/ame]
From R/L, sr 4140 blast baffle on to the muzzle. I didnt ask how many rounds
I had hoped I was cutting a fat hog with the cryo. I also had a .22 can have the baffles collapse in FA because I was trying to cut them too thin. They work great on a reg. .22 though
Last edited: